Spinellisation Study of Three Different Mg0-AI20 3 Compositions Using a Dilatometer
Ritwik Sarkar, Goutam Banerjee* and Tapan Kr. Pal
Pages : 173-175
DOi : 10.1080/0371750X.2002.10800057
Abstract
Three different Mg0-AI20 3 spinel compositions having MgO : Al 20 3 molar ratios 2 : 1, 1 : 1 and 1 : 2 have been studied. Isostatically pressed green compacts of oxide mixtures were used for the dilatometric study and a maximum temperature of 1400°C was used. Dilatometric study reveals that the formation of spinel starts above 1000°C for all the compositions and the linear expansion values are in good agreement with their expected values considering theoretically possible (maximum) spinel content. The fall in expansion values was also observed at and above 1350°C due to greater shrinkage rate (from sintering) than the rate of expansion from spinellisation. The phase analyses of the final products showed spinel as the major phase with some free oxides due to incomplete spinellisation reaction.
Full text : Subscribe to Download Full Text
[Go Back]
 
MAIN PAGE | SITE MAP | PRIVACY POLICY | TERMS & CONDITIONS  | CONTACT US | FEEDBACK
Copyright © 2008-2026 The Indian Ceramic Society. All Rights Reserved

Managed by : htsm