Thermal Endurance Studies on Some Fired Saggar Bodies
s. K. GUHA, s. CHATTERJEE AND A. DAS GUPTA
Pages : 209-211
DOI : 10.1080/0371750X.1981.1082255
Abstract
Clay-based saggars, commonly used in the pottery industries in India, can not stand more than 5 to 6 thermal cycles. With a view to understanding the different parameters controlling the thermal shock resistance property of fired ceramics, b!ldies containing 50% cordierite grog-50% clay, 50% clay grog-50% clay and 50% cl~y grog- 50% cordierite were prepared with variations in grog s1zes. The strength was measured after each thermal cycle. From the studies, it could be inferred that by using preformed cordierite, much longer life would be assured and a method for evaluating thermal endurance of fired ceramics could be standardised.
Full text : Subscribe to Download Full Text
[Go Back]
 
MAIN PAGE | SITE MAP | PRIVACY POLICY | TERMS & CONDITIONS  | CONTACT US | FEEDBACK
Copyright © 2008-2026 The Indian Ceramic Society. All Rights Reserved

Managed by : htsm