As reported earlier, electrical conductivity of sintered uranium dioxide pellets depended on the calcination temperature and the sintering treatments, and could be related to the microstructure attained. The highest sintering temperature studied was J70rJC. In the present study, high density pellets prepared by sintering at 1500°C were refired at 1800°, 1900° and 2000°C. Though there were no significant changes in the densities, the electrical conductivity of the samples varied considerably showing a minima at a refiring temperature of 1900°C. Attempts were made to correlate the changes in electrical conductivity to the microstructural changes llhich still seem to be influenced by the thermal history of the samples.
Full text : Subscribe to Download Full Text
[Go Back]
 
MAIN PAGE | SITE MAP | PRIVACY POLICY | TERMS & CONDITIONS  | CONTACT US | FEEDBACK
Copyright © Protected 2008, The Indian Ceramic Society. All right reserved.

Developed By : Hi-Tech Soft & Multimedia